Product Details:
Place of Origin: CHINA
Brand Name: EASTKING
Certification: ISO/SGS
Model Number: PFA
Payment & Shipping Terms:
Minimum Order Quantity: 1MT
Price: USD500-800/MT
Packaging Details: 1MT/bag, 1.25MT/bag, 25kg bags into 1MT big bag, on pallet
Delivery Time: 7days for quantity within 1000MT
Payment Terms: T/T, L/C, D/A, D/P, , MoneyGram
Supply Ability: 2600MT/Month

Roller Crushed Pink Fused Alumina 30# Tougher For Bonded Grinding Wheels

Description
Product Name: Pink Fused Alumina 99.2% Application: Bonded Grinding Abrasives
Al2O3 Content: 99.2% Size: Customer Requirements
Hardness: 9.0 Mohs Shape: Grit(Equaled Volume)
High Light:

Roller Crushed Pink Fused Alumina

,

30# Pink Fused Alumina

,

30# Pink Aluminum Oxide

Durable Barmac Crushed Pink Fused Alumina 30# for Bonded Grinding Wheels

 

1. Pink Fused Alumina Introduction

 

Pink Fused Alumina is produced by doping Chromia into Alumina, which gives the material pink color. The incorporation of the Cr2O3 into the AI2O3 crystal lattice produces a slight increase in toughness and a reduced friability compared with white Fused Alumina.
Compared to Brown Regular Aluminum Oxide the Pink material is harder, more aggressive and has better cutting ability. The grain shape of Pink Aluminum Oxide is sharp and angular.

 

2. Pink Fused AluminaSpecifications

 

Items / Chemical Composition Unit Medium Chrome Low Chrome High Chrome
Size F12-F80 AI2O3 % 98.2 min 98.5 min 97.4 min
Cr2O3 % 0.45-1.00 0.20-0.45 1.00-2.00
Na2O % 0.55 max 0.50 max 0.55 max
F90-F150 AI2O3 % 98.20 min 98.50 min 97.00 min
Cr2O3 % 0.45-1.00 0.20-0.45 1.00-2.00
Na2O % 0.60 max 0.50 max 0.60 max
F180-F220 AI2O3 % 97.80 min 98.00 min 96.50 min
Cr2O3 % 0.45-1.00 0.20-0.45 1.00-2.00
Na2O % 0.70 max 0.60 max 0.70 max
Physical Property Basic Minerals   α-AI2O3 α-AI2O3 α-AI2O3
Crystal Size µ m 600~2000 600~2000 600~2000
True Density g/cm3 > 3.90 > 3.90 > 3.90
Bulk Density g/cm3 1.40~1.91 1.40~1.91 1.40~1.91
Knoop Hardness g/cm3 2200~2300 2200~2300 2200~2300

 

3. Pink Fused Alumina General advantages

 

1. High hardness;

2. Sharp edges;

3. Outstanding durability;

4. High toughness;

5. Sharper and stronger than brown aluminum oxide;

6. Practically zero iron content.

 

4. Pink Fused Alumina Characteristics

 

1. High toughness;

2. high hardness;

3. good self-sharpening;

3. Environmental protection;

4. Strong grinding ability and Low heat generation.

 

5. Pink Fused Alumina Applications

 

The FEPA F grades are especially suitable for the manufacturing vitrified bonded abrasives for working hardened steels and alloys with tensile strengths of over 50 Kg/mm2. It is also used in tool grinding, knife - sharpening applications, precision grinding, profile grinding, flute grinding, tooth grinding, dry grinding of blade segments and mounted wheels. The FEPA P grades are a preferred material for working non-ferrous metals and the alloys (copper, aluminium, zinc, brass, Bronze), but also used for softer materials, such as wood, synthetics and pains.

 

Roller Crushed Pink Fused Alumina 30# Tougher For Bonded Grinding Wheels 0Roller Crushed Pink Fused Alumina 30# Tougher For Bonded Grinding Wheels 1

Contact Details
Eastking Industrial Limited

Contact Person: Jason Chen

Tel: 86-18603794999

Send your inquiry directly to us (0 / 3000)